- Introduction
Introduction
Usage
It is suitable for long-distance transportation of bulk materials, used in mines, ports, electricity, metallurgy, chemical industries, coalmines, etc.
Characteristics
1. When a running belt is pieced and sensor loop embedded in belt is damaged, including the belt is torn, the signal control system will shut down the machine automatically and sound the alarm, so that the torn degree of the belt will be minimized.
2. When the conveyor belt deviates in running, the distance between the sensor loop embedded in the belt and sensor exceeds the set value, the signal control system will shut down the machine automatically and sound the alarm.
3. When the materials are jammed, the sensor will detect the abnormal running speed of the belt, the signal control system will shut down the machine automatically and sound the alarm.
4. The running state of the conveyor belt can be monitored through network at any time in any place.
Standard Specifications
Model | Tensile Strength(N/mm) | Cord Pitch (mm) | Cord Diameter (mm) | Min Cover thickness (mm) | Width (mm) |
ST630 | 630 | 10 | 3 | 4 | 800-2400 |
ST800 | 800 | 10 | 3.5 | 4 | |
ST1000 | 1000 | 12 | 4 | 4 | |
ST1250 | 1250 | 12 | 4.5 | 4 | |
ST1600 | 1600 | 12 | 5 | 4 | |
ST2000 | 2000 | 12 | 6 | 4 | |
ST2500 | 2500 | 15 | 7.2 | 5 | |
ST3150 | 3150 | 15 | 8.1 | 5.5 | |
ST3500 | 3500 | 15 | 8.6 | 6 | |
ST4000 | 4000 | 15 | 8.9 | 6.5 | |
ST4500 | 4500 | 16 | 9.7 | 7 | |
ST5000 | 5000 | 17 | 10.9 | 7.5 | |
ST5400 | 5400 | 17 | 11.3 | 8 | |
ST6300 | 6300 | 19.5 | 12.8 | 10 | |
ST7000 | 7000 | 19.5 | 13.5 | 10 | |
ST7500 | 7500 | 21 | 15 | 10 |
Note: Cover thickness, cord diameter, and cord pitch can be manufactured according to customer’s requirements.
Cover Grades
Grade | Tensile Strength(ISO37) Mpa | Elongation at break min. (ISO37) % | Abrasion max. (ISO4649) mm³ |
H | 24 | 450 | 120 |
D | 18 | 400 | 100 |
XTO D | 18 | 400 | 50 |
The values will help to determine the appropriate cover compound for the application or for the materials carries. Reliable assessment of the behavior of the covers in service for wear and cut resistance cannot be determined from tensile strength, and abrasion values alone.